Jun. 2005
2-component type. Semi-gloss finish.
ABS, thermosetting resin(phenol, epoxy), primed metal, organic surface of engineering plastics(nylon, PPS, liquid crystal polymer). When drying at low temperature is required in the printing on inorganic substrate such as primed metal, aluminum, steel, stainless or copper, this usage should be taken.
Hardener : | Add JA-960 by 10-20%. Small addition leads to flexible ink film and good adhesion. Larger addition leads to hard ink film and good alcohol resistance. |
|
Thinner : | Add E THINNER or NT THINNER(fast drying, standard drying, slow drying)to the mixture by 5-20%. Stir well before use. | |
Drying : | 70°C(158°F) 30-120 min(ABS) or 100°C(212°F) 60 min or 120°C(248°F) 12 min. The relationship between drying time and alcohol resistance |
Drying time in 70°C(158°F) |
30 min. |
60 min. |
120 min. |
---|---|---|---|
alcohol resistance (rubbing times with 95% ethanol) |
30-60 | 100-200 | 200-400 |
Pot life : | 6-8 hours at 20°C(68°F). Ink still has its fluidity after pot life. However, it is advised not to use it as properties degrade. | |
Washing : | Use our #10 CLEANING THINNER. |
When it is possible to bake at high temperature in the printing on inorganic substrate such as primed metal, aluminum, steel, stainless or copper, this usage should be taken.
Hardener : | Add JA-1000 by 1-3%. | |
Thinner : | Add E THINNER or NT THINNER(fast drying, standard drying, slow drying)to the mixture by 5-20%. Stir well before use. | |
Drying : | 100°C(212°F) 60 min or 120°C(248°F) 20 min or 150°C(302°F) 5 min. | |
Pot life : | 12 hours at 20°C(68°F). Ink still has its fluidity after pot life. However, it is advised not to use it as properties degrade. | |
Washing : | Use our #10 CLEANING THINNER. |
07 opaque white, 13 lemon yellow, 14 yellow, 28 orange, 06 bright red, 08 red, 18 geranium, 16 pink, 25 violet, 45 deep blue, 46 blue, 75 green, 90 black, 00 clear
Ink : 1kg can.
Hardener : 0.1kg plastic container.
Thinner : 1kg can